Differential Scanning Calorimeter Netzsch DSC 204 F1 Phoenix

Measurements of calorimetric properties, e.g

  • example reaction temperatures,
  • crystallization,
  • specific heat capacity,
  • heat of fusion,
  • thermal stability,
  • glass transition,
  • oxidative induction temperature,
  • oxidative induction time, 

  • temperature range   -180°C to 700°C   
  • heating rate    0,001K/min to 200K/min   
  • high cooling rate: max. 200K/min   
  • gas tight cell   